Title: | Effect of iron doping on the properties of nanopowders and coatings on the basis of Al2O3 produced by pulsed electron beam evaporation |
Authors: | Sokovnin, S. Y. Il'ves, V. G. Surdo, A. I. Mil'man, I. I. Vlasov, M. I. |
Issue Date: | 2013 |
Citation: | Effect of iron doping on the properties of nanopowders and coatings on the basis of Al2O3 produced by pulsed electron beam evaporation / S. Y. Sokovnin, V. G. Il'ves, A. I. Surdo [et al.] // Nanotechnologies in Russia. — 2013. — Vol. 8. — № 7-8. — P. 466-481. |
Abstract: | Multiphase nanopowders (NPs) and amorphous/amorphous-nanocrystalline coatings (A-NC) have been prepared by the evaporation of ceramic targets of Al2O3-Fe2O3 (0.1, 3, 5 Fe2O3 mass %) by a pulsed electron beam in vacuum. The specific surface area of NP Al2O3-Fe2O3 reached 277 m2/g. The α and γ phases Al2O3 and other nonidentified phases have been found in the composition of NP Al2O3-Fe2O3. All coatings contained an insignificant fraction of the crystalline γ phase. No secondary phases on the basis of iron have been revealed. According to transmission electron microscopy, the fine fraction of NP Al2O3-Fe2O3 consists of amorphous nanoparticles of an irregular and quasispherical shape no more than 10 nm in size which form agglomerates reaching 1.5 μm. A large fraction of NPs consists of crystal spherical nanoparticles with preferential sizes of about 10-20 nm. All NP Al2O3-Fe2O3 showed ferromagnetic behavior at room temperature. The maximum magnetic response has been established in NPs with a minimum iron content (1.1 mass %). The pulsed cathode luminescence spectra of coatings and NP Al2O3-Fe2O3 have been presented by a wide band in the wavelength range of 300-900 nm regardless of their phase composition. Phase transformations into NP AL2O3-1.1% Fe and coatings from undoped Al2O3 heated to 1400°C occur according to the following scheme: amorphous phase → γ → δ → θ → α, regardless of their initial phase composition. The threshold of thermal stability of the Γ phase in NPs and the coating of undoped Al2O3 does not exceed 830°C. For the first time, the increased thermo and optically stimulated luminescent response comparable with the response of the leading TLD-500K thermoluminescent dosimeter has been reached in A-NC coatings of undoped Al2O3. © 2013 Pleiades Publishing, Ltd. |
Keywords: | AMORPHOUS NANOPARTICLES CATHODE LUMINESCENCE FERROMAGNETIC BEHAVIORS MAGNETIC RESPONSE PULSED ELECTRON BEAMS SPHERICAL NANOPARTICLES THERMOLUMINESCENT DOSIMETERS WAVELENGTH RANGES ALUMINUM COATINGS ELECTRON SOURCES LUMINESCENCE NANOPARTICLES NANOSTRUCTURED MATERIALS PHASE COMPOSITION PHASE TRANSITIONS TRANSMISSION ELECTRON MICROSCOPY VACUUM EVAPORATION ALUMINUM COATINGS |
URI: | http://elar.urfu.ru/handle/10995/27076 |
SCOPUS ID: | 84881509042 |
PURE ID: | 900808 |
ISSN: | 1995-0780 |
DOI: | 10.1134/S1995078013040186 |
Appears in Collections: | Научные публикации ученых УрФУ, проиндексированные в SCOPUS и WoS CC |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
scopus-2013-0253.pdf | 912,61 kB | Adobe PDF | View/Open |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.