Title: | Shape of isolated domains in lithium tantalate single crystals at elevated temperatures |
Authors: | Shur, V. Ya. Akhmatkhanov, A. R. Chezganov, D. S. Lobov, A. I. Baturin, I. S. Smirnov, M. M. Шур, В. Я. |
Issue Date: | 2013 |
Citation: | Shape of isolated domains in lithium tantalate single crystals at elevated temperatures / V. Ya. Shur, A. R. Akhmatkhanov, D. S. Chezganov [et al.] // Applied Physics Letters. — 2013. — Vol. 103. — № 24. |
Abstract: | The shape of isolated domains has been investigated in congruent lithium tantalate (CLT) single crystals at elevated temperatures and analyzed in terms of kinetic approach. The obtained temperature dependence of the growing domain shape in CLT including circular shape at temperatures above 190 °C has been attributed to increase of relative input of isotropic ionic conductivity. The observed nonstop wall motion and independent domain growth after merging in CLT as opposed to stoichiometric lithium tantalate have been attributed to difference in wall orientation. The computer simulation has confirmed applicability of the kinetic approach to the domain shape explanation. © 2013 AIP Publishing LLC. |
Keywords: | CIRCULAR SHAPE ELEVATED TEMPERATURE GROWING DOMAINS KINETIC APPROACH LITHIUM TANTALATE STOICHIOMETRIC LITHIUM TANTALATES TEMPERATURE DEPENDENCE WALL ORIENTATION COMPUTER SIMULATION SINGLE CRYSTALS LITHIUM |
URI: | http://elar.urfu.ru/handle/10995/26863 |
SCOPUS ID: | 84890505158 |
WOS ID: | 000328706500065 |
PURE ID: | 835877 |
ISSN: | 0003-6951 |
DOI: | 10.1063/1.4846015 |
Appears in Collections: | Научные публикации ученых УрФУ, проиндексированные в SCOPUS и WoS CC |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
scopus-2013-0099.pdf | 1,1 MB | Adobe PDF | View/Open |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.