Please use this identifier to cite or link to this item: http://elar.urfu.ru/handle/10995/120157
Title: Dilatometric characteristics of weakly sintered ceramics
Authors: Komolikov, Yu. I.
Ermakova, L. V.
Khrustov, V. R.
Zhuravlev, V. D.
Issue Date: 2022-12
Publisher: Ural Federal University
Уральский федеральный университет
Citation: Dilatometric characteristics of weakly sintered ceramics / Yu. I. Komolikov, L. V. Ermakova, V. R. Khrustov, V. D. Zhuravlev // Chimica Techno Acta. — 2022. — Vol. 9, No. 4. — № 20229412.
Abstract: Thermal expansion of refractory ceramics CaZrO3, MgAl2O4, La2Zr2O7 and YSZ-12 was studied. The samples of the complex oxides were synthesized by solution combustion synthesis with glycine; the fuel:oxidant ratio was varied depending on the character of redox reaction. The linear thermal expansion coefficient (LTEC) of ceramics was measured on the samples with an initial density 23–52%. The maximal sinterability of 89–92% after 6 h annealing at 1550 °С was demonstrated by La2Zr2O7 and YSZ-12, and the minimal values (78–82%) – by CaZrO3 and MgAl2O4. All materials have close LTEC values, from 9.0 to 9.6·10–6 K–1.
Keywords: REFRACTORY OXIDE
WEAKLY SINTERED CERAMICS
LINEAR THERMAL EXPANSION
COEFFICIENT THERMAL EXPANSION
CERAMIC DENSITY
URI: http://elar.urfu.ru/handle/10995/120157
RSCI ID: https://www.elibrary.ru/item.asp?id=50082609
ISSN: 2411-1414
DOI: 10.15826/chimtech.2022.9.4.12
Sponsorship: This study was carried out in the framework of the state assignment for the Institute of Solid State Chemistry UB RAS (No. АААА-А19-119031890026-6), Mikheev Institute of Metal Physics UB RAS (No. АААА-А18-118020690196-3) and the Institute of Electrophysics UB RAS (No. 122011200363-9).
Origin: Chimica Techno Acta. 2022. Vol. 9. № 4
Appears in Collections:Chimica Techno Acta

Files in This Item:
File Description SizeFormat 
cta-2022-4-13.pdf402,14 kBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.