Пожалуйста, используйте этот идентификатор, чтобы цитировать или ссылаться на этот ресурс: http://elar.urfu.ru/handle/10995/90140
Полная запись метаданных
Поле DCЗначениеЯзык
dc.contributor.authorLoginov, Y. N.en
dc.contributor.authorPervukhin, A. E.en
dc.contributor.authorBabailov, N. A.en
dc.date.accessioned2020-09-29T09:46:09Z-
dc.date.available2020-09-29T09:46:09Z-
dc.date.issued2017-
dc.identifier.citationLoginov, Y. N. Evolution of surface defects in platinum alloy wire under drawing / Y. N. Loginov, A. E. Pervukhin, N. A. Babailov. — DOI 10.1063/1.5017380 // AIP Conference Proceedings. — 2017. — Iss. 1915. — 40032.en
dc.identifier.isbn9780735416079-
dc.identifier.issn0094-243X-
dc.identifier.otherhttps://aip.scitation.org/doi/pdf/10.1063/1.5017380pdf
dc.identifier.other1good_DOI
dc.identifier.other3c491fa6-7834-4015-ba4e-b480f18a7b08pure_uuid
dc.identifier.otherhttp://www.scopus.com/inward/record.url?partnerID=8YFLogxK&scp=85038931872m
dc.identifier.urihttp://elar.urfu.ru/handle/10995/90140-
dc.description.abstractThe shape and chemical composition of particles polluting the surface of ultrafine wire made of the platinum Pt92.5Pd4Rh3.5 alloy has been revealed by electron microscopy and microspectral analysis. The phenomenon of the appearance of pores in the particles, which are elongated in the direction of drawing, has been discovered. The problem of calculating the stress-strain state is stated by the finite element method. After solving the problem, it is demonstrated that the appearance of additional defects is related to the proportion of stresses in the scheme of metal forming by drawing. © 2017 Author(s).en
dc.description.sponsorshipThe work was done within the State Task, theme No. 01201375904, and financially supported by the RF Government, No. 211 (contract No. 02.A03.21.0006).en
dc.format.mimetypeapplication/pdfen
dc.language.isoenen
dc.publisherAmerican Institute of Physics Inc.en
dc.rightsinfo:eu-repo/semantics/openAccessen
dc.sourceAIP Conference Proceedingsen
dc.titleEvolution of surface defects in platinum alloy wire under drawingen
dc.typeConference Paperen
dc.typeinfo:eu-repo/semantics/conferenceObjecten
dc.typeinfo:eu-repo/semantics/publishedVersionen
dc.identifier.doi10.1063/1.5017380-
dc.identifier.scopus85038931872-
local.affiliationUral Federal University Named after the First President of Russia B. N. Yeltsin, 19 Mira St., Ekaterinburg, 620002, Russian Federationen
local.affiliationInstitute of Engineering Science, Ural Branch, Russian Academy of Sciences, 34 Komsomolskaya St., Ekaterinburg, 620049, Russian Federationen
local.contributor.employeeLoginov, Y.N., Ural Federal University Named after the First President of Russia B. N. Yeltsin, 19 Mira St., Ekaterinburg, 620002, Russian Federationru
local.contributor.employeePervukhin, A.E., Ural Federal University Named after the First President of Russia B. N. Yeltsin, 19 Mira St., Ekaterinburg, 620002, Russian Federationru
local.contributor.employeeBabailov, N.A., Institute of Engineering Science, Ural Branch, Russian Academy of Sciences, 34 Komsomolskaya St., Ekaterinburg, 620049, Russian Federationru
local.issue1915-
dc.identifier.wos000423872300068-
local.identifier.pure6251761-
local.description.order40032-
local.identifier.eid2-s2.0-85038931872-
local.identifier.wosWOS:000423872300068-
Располагается в коллекциях:Научные публикации ученых УрФУ, проиндексированные в SCOPUS и WoS CC

Файлы этого ресурса:
Файл Описание РазмерФормат 
10.1063-1.5017380.pdf1,08 MBAdobe PDFПросмотреть/Открыть