Пожалуйста, используйте этот идентификатор, чтобы цитировать или ссылаться на этот ресурс: http://elar.urfu.ru/handle/10995/141752
Название: Assessment of homogeneity of ladle-furnace refining slag by calculation and experimental methods; [Оценка гомогенности рафинировочного шлака АКП расчетным и экспериментальным методами]
Авторы: Murysev, V. A.
Sheshukov, O. Y.
Safonov, V. M.
Somov, S. A.
Metelkin, A. A.
Egiazar’yan, D. K.
Дата публикации: 2024
Издатель: National University of Science and Technology MISIS
Библиографическое описание: Мурысев, В. А., Шешуков, О. Ю., Сафонов, В. М., Сомов, С. А., Метелкин, А. А., & Егиазарьян, Д. К. (2024). Оценка гомогенности рафинировочного шлака АКП расчетным и экспериментальным методами. Известия высших учебных заведений. Черная металлургия, 67(2), 140-147. https://doi.org/10.17073/0368-0797-2024-2-140-147
Аннотация: The paper considers the issues of determining undissolved CaO and MgO particles in slags formed in a ladlefurnace unit. The assessment of slags by the presence and quantity of undissolved oxides CaO and MgO, depending on chemical composition, was carried out using a polymer model developed at UrFU and improved at IMeT UrB RAS. To determine the saturation of a multicomponent melt by CaO and MgO oxides, it is necessary to compare two parameters: thermodynamic activity of oxide in the melt, which depends on chemical composition, and saturation activity, which depends on temperature. The authors propose a method for estimating the content of undissolved particles in the slags formed at the steel ladle treatment at JSC VMZ. Most slags contain undissolved lime in an amount less than 10 %, which is sufficient for successful steel desulfurization. Theoretical calculations for determination of undissolved particles were confirmed in laboratory conditions during studies of industrial slags with a Stengelmeyer viscometer. Laboratory experiments showed the accuracy of the calculated method for determining the solid phase in the slags formed in ladlefurnace unit by comparing the viscosity changes with a decrease in the slags temperature. Solidification temperature of heterogeneous slag is 200 °C higher than that of homogeneous one. When temperature of heterogeneous slag decreased, enlarged agglomerates of solid oxides were formed, which fell under the measuring device, respectively, it showed an increased viscosity of the oxide system in the temperature range of 1570 – 590 °C. Laboratory experiments confirm the methodology for determining the solid phase in the slag. © 2024 National University of Science and Technology MISIS. All rights reserved.
Ключевые слова: HETEROGENEOUS SLAG
HOMOGENEOUS SLAG
LADLEFURNACE UNIT
LIME DISSOLUTION
SLAG
UNDISSOLVED PARTICLES
VISCOMETER
URI: http://elar.urfu.ru/handle/10995/141752
Условия доступа: info:eu-repo/semantics/openAccess
cc-by
Идентификатор РИНЦ: 67219593
Идентификатор SCOPUS: 85192737993
Идентификатор PURE: 57314527
ISSN: 2410-2091
0368-0797
DOI: 10.17073/0368-0797-2024-2-140-147
Располагается в коллекциях:Научные публикации ученых УрФУ, проиндексированные в SCOPUS и WoS CC

Файлы этого ресурса:
Файл Описание РазмерФормат 
2-s2.0-85192737993.pdf875,69 kBAdobe PDFПросмотреть/Открыть


Все ресурсы в архиве электронных ресурсов защищены авторским правом, все права сохранены.