Название: | Composite Electrochemical Coatings of Ni-CrB2 from Sulfuric Acid and Sulfamate Electrolytes: Formation, Structure and Properties |
Авторы: | Petukhova, P. M. Bushueva, E. G. Novgorodtseva, O. N. |
Дата публикации: | 2024 |
Издатель: | Уральский федеральный университет Ural Federal University |
Библиографическое описание: | Petukhova P. M. Composite Electrochemical Coatings of Ni-CrB2 from Sulfuric Acid and Sulfamate Electrolytes: Formation, Structure and Properties / P. M. Petukhova, E. G. Bushueva, O. N. Novgorodtseva // Chimica Techno Acta. — 2024. — Vol. 11, No. 4. — № 202411406. |
Аннотация: | Electrodeposited coatings are in demand in many industries: due to the high adhesive strength to the base metal, they can be applied to complexshaped products, and the thickness of the deposited coating can be controlled. However, standard electrolytic coatings do not always meet the necessary operating requirements. In this case, the formation of composite electrolytic coatings, which consist in the modification of electrolytes by various dispersed particles, becomes an urgent task. These particles are introduced into the electrolyte and deposited together with the precipitate metals, which leads to changes in the coating properties. In this article, the structure, adhesive and corrosion properties of nickel-chromium diboride composite coatings obtained in the electrodeposition process are studied. Precipitation was carried out in sulfuric acid and sulfamate electrolytes with a concentration of dispersed chromium diboride particles of 10-40 g/l. The coatings consist of nickel and CrB2 phases. The adhesive strength of the coating with a steel base is satisfactory; chipping and peeling were not observed. The corrosion resistance of sulfamate electrolyte coatings is higher than that of the coatings obtained from sulfuric acid electrolyte due to the compactness of nickel precipitates. Chromium diboride in the coating provides 1.5-2 times greater corrosion resistance. |
Ключевые слова: | ELECTRODEPOSITION NICKEL PLATING COMPOSITE ELECTROLYTIC COATINGS CHROMIUM DIBORIDE CORROSION RESISTANCE |
URI: | http://elar.urfu.ru/handle/10995/140711 |
Идентификатор РИНЦ: | https://elibrary.ru/item.asp?id=79391889 |
ISSN: | 2411-1414 |
DOI: | 10.15826/chimtech.2024.11.4.06 |
Сведения о поддержке: | The work was carried out in accordance with the state task of the Ministry of Education and Science of Russia (project FSUN-2023-0009). |
Источники: | Chimica Techno Acta. 2024. Vol. 11. № 4 |
Располагается в коллекциях: | Chimica Techno Acta |
Файлы этого ресурса:
Файл | Описание | Размер | Формат | |
---|---|---|---|---|
cta-2024-4-06.pdf | 477,89 kB | Adobe PDF | Просмотреть/Открыть |
Все ресурсы в архиве электронных ресурсов защищены авторским правом, все права сохранены.