Название: Revealing Lithiation Kinetics and Battery Degradation Pathway in LiMn2O4-Based Commercial Cathodes via Electrochemical Strain Microscopy
Авторы: Alikin, D.
Slautin, B.
Kholkin, A.
Дата публикации: 2022
Издатель: MDPI
Библиографическое описание: Alikin, D, Slautin, B & Kholkin, A 2022, 'Revealing Lithiation Kinetics and Battery Degradation Pathway in LiMn2O4-Based Commercial Cathodes via Electrochemical Strain Microscopy', Batteries, Том. 8, № 11, 220. https://doi.org/10.3390/batteries8110220
Alikin, D., Slautin, B., & Kholkin, A. (2022). Revealing Lithiation Kinetics and Battery Degradation Pathway in LiMn2O4-Based Commercial Cathodes via Electrochemical Strain Microscopy. Batteries, 8(11), [220]. https://doi.org/10.3390/batteries8110220
Аннотация: The capacity fade during the cycling of lithium batteries is a key factor limiting further progress in the improvement of electric vehicles, wearable electronic devices, alternative energy sources, etc. One of the main reasons for capacity loss is battery cathode degradation, which significantly influences the battery lifetime. Despite in-depth knowledge of battery degradation at the chemical level, the kinetics of the degradation at the resolution of the individual elements of the cathode are not fully understood. Here, we studied lithiation kinetics in commercial cathodes based on lithium manganese spinel using the electrochemical strain microscopy local method. Supported by the experimental finding, the “viscous fingers” model of lithium ions intercalation–deintercalation in individual particles of the cathode was proposed. The non-linear dynamics of the lithiation front were suggested to be stimulated by the non-uniform stress field and gradient of the chemical potential. Irregularity of the lithiation front causes the formation of the residual lithiated pocket in the delithiated particles, which effectively reduces the volume available for chemical reaction. The obtained results shed further light on the degradation of the lithium battery cathodes and can be applicable for other cathode materials. © 2022 by the authors.
Ключевые слова: INTERCALATION KINETICS
LITHIATION REACTION
NANOSCALE RESOLUTION
VISCOUS FINGERS
DEGRADATION
ELECTRIC LOSSES
INTERCALATION
KINETICS
LITHIUM-ION BATTERIES
REACTION KINETICS
BATTERY DEGRADATION
CAPACITY FADE
DEGRADATION PATHWAYS
ELECTROCHEMICAL STRAIN MICROSCOPIES
INTERCALATION KINETICS
KEY FACTORS
LITHIATION
LITHIATION REACTION
NANOSCALE RESOLUTIONS
VISCOUS FINGERS
CATHODES
URI: http://elar.urfu.ru/handle/10995/131335
Условия доступа: info:eu-repo/semantics/openAccess
cc-by
Текст лицензии: https://creativecommons.org/licenses/by/4.0/
Идентификатор SCOPUS: 85141782109
Идентификатор WOS: 000883859600001
Идентификатор PURE: 31787768
2d2af7aa-63c2-458c-afa2-9b1b9cc55fd5
ISSN: 2313-0105
DOI: 10.3390/batteries8110220
Сведения о поддержке: Ministry of Education and Science of the Russian Federation, Minobrnauka
Ministry of Science and Higher Education of the Russian Federation, (075-15-2021-677)
Funding text 1: The equipment of the Ural Center for Shared Use “Modern nanotechnology” of Ural Federal University (Reg. # 2968), which is supported by the Ministry of Science and Higher Education RF (Project # 075-15-2021-677), was used.
Funding text 2: The research funding from the Ministry of Science and Higher Education of the Russian Federation (Ural Federal University Program of Development within the Priority-2030 Program) is gratefully acknowledged.
Располагается в коллекциях:Научные публикации ученых УрФУ, проиндексированные в SCOPUS и WoS CC

Файлы этого ресурса:
Файл Описание РазмерФормат 
2-s2.0-85141782109.pdf2,63 MBAdobe PDFПросмотреть/Открыть


Лицензия на ресурс: Лицензия Creative Commons Creative Commons