Название: | Experimental assessment for the photon shielding features of silicone rubber reinforced by tellurium borate oxides |
Авторы: | Elsafi, M. ALasali, H. J. Almuqrin, A. H. Mahmoud, K. G. Sayyed, M. I. |
Дата публикации: | 2023 |
Издатель: | Korean Nuclear Society |
Библиографическое описание: | Elsafi, M, Alasali, HJ, Almuqrin, AH, Mahmoud, KG & Sayyed, MI 2023, 'Experimental assessment for the photon shielding features of silicone rubber reinforced by tellurium borate oxides', Nuclear Engineering and Technology, Том. 55, № 6, стр. 2166-2171. https://doi.org/10.1016/j.net.2023.02.022 Elsafi, M., Alasali, H. J., Almuqrin, A. H., Mahmoud, K. G., & Sayyed, M. I. (2023). Experimental assessment for the photon shielding features of silicone rubber reinforced by tellurium borate oxides. Nuclear Engineering and Technology, 55(6), 2166-2171. https://doi.org/10.1016/j.net.2023.02.022 |
Аннотация: | In the present study, six silicone rubber doped by tellurium borate oxides were fabricated using the casting method. The densities of the fabricated silicon rubber-doped by tellurium borate oxides samples were measured using the Archimedes Method. Moreover, the linear attenuation coefficient of silicone rubber doped tellurium borate oxides samples was evaluated experimentally using the hyper pure germanium, and the recorded linear attenuation coefficient values were affirmed using the theoretical Phy-X program. The experimental measurements were performed using the narrow beam transmission method with radioactive isotopes Am-241, Cs-137, and Co-60 with energies of 59, 661, 1173, and 1332 keV. The linear attenuation coefficient values showed an enhancement by 4.73 times, 1.20 time, 1.17, time, and 1.17 time, respectively at gamma photon energies of 59, 661, 1173, and 1332 keV, when the TeO2 concentration increased in the fabricated composites from 0 to 50 wt%. The enhancement of the linear attenuation coefficient values has a positive effect on the transmission rate values where the half-value thickness and transmission rate were decreased accompanied by an increase in the RPE. © 2023 Korean Nuclear Society |
Ключевые слова: | BORATE OXIDE HYPER PURE GERMANIUM SILICONE RUBBER TELLURIUM OXIDE |
URI: | http://elar.urfu.ru/handle/10995/130477 |
Условия доступа: | info:eu-repo/semantics/openAccess cc-by-nc-nd |
Текст лицензии: | https://creativecommons.org/licenses/by-nc-nd/4.0/ |
Идентификатор SCOPUS: | 85159192144 |
Идентификатор WOS: | 001003019300001 |
Идентификатор PURE: | 39238889 |
ISSN: | 1738-5733 |
DOI: | 10.1016/j.net.2023.02.022 |
Сведения о поддержке: | Princess Nourah Bint Abdulrahman University, PNU: PNURSP2023R2 The authors express their gratitude to the Princess Nourah bint Abdulrahman University Researchers Supporting Project number (PNURSP2023R2), Princess Nourah bint Abdulrahman University, Riyadh, Saudi Arabia. |
Располагается в коллекциях: | Научные публикации ученых УрФУ, проиндексированные в SCOPUS и WoS CC |
Файлы этого ресурса:
Файл | Описание | Размер | Формат | |
---|---|---|---|---|
2-s2.0-85159192144.pdf | 1,54 MB | Adobe PDF | Просмотреть/Открыть |
Лицензия на ресурс: Лицензия Creative Commons