dc.contributor.author | Космацкий, Я. И. | ru |
dc.contributor.author | Водолазский, Ф. В. | ru |
dc.contributor.author | Горностаева, Е. А. | ru |
dc.contributor.author | Илларионова, С. М. | ru |
dc.contributor.author | Ширинкина, Н. А. | ru |
dc.contributor.author | Kosmatskii, Ia. I. | en |
dc.contributor.author | Vodolazskii, F. V. | en |
dc.contributor.author | Gornostaeva, E. A. | en |
dc.contributor.author | Illarionova, S. M. | en |
dc.contributor.author | Shirinkina, N. A. | en |
dc.date.accessioned | 2023-10-10T08:19:56Z | - |
dc.date.available | 2023-10-10T08:19:56Z | - |
dc.date.issued | 2022-08-17 | - |
dc.identifier.uri | http://elar.urfu.ru/handle/10995/127259 | - |
dc.description.abstract | Изобретение относится к металлургии, а именно к изготовлению бесшовных холоднодеформированных труб из титановых сплавов, и может быть использовано для изготовления изделий ответственного назначения. Способ изготовления холоднодеформированных бесшовных труб из титановых сплавов включает механическую обработку горячедеформированных цилиндрических заготовок, прессование, правку и механическую обработку полученных горячепрессованных труб, последующую многопроходную холодную прокатку при осуществлении промежуточных термических обработок в вакууме в зависимости от сплава и конечную термическую обработку труб готового размера в вакууме. В качестве титановых сплавов для труб используют сплав ПТ-1М или ПТ-7М, перед нагревом под прессование на поверхность заготовок наносят защитное покрытие, представляющее собой шликерную обмазку, состоящую из смеси порошка эмали ЭВТ-24, молотой бентонитовой глины и жидкого стекла. Далее осуществляют прессование при температуре Т<sub>Н</sub>, которую определяют по зависимости: Т<sub>Н</sub> = Т<sub>ПП</sub> – k⋅ε⋅υ<sub>ПР</sub>, где Т<sub>ПП</sub> – температура полиморфного превращения, °С; k – эмпирический коэффициент, учитывающий влияние деформационного разогрева, °С·с/мм; для сплава ПТ-1М эмпирический коэффициент k от 0,035 до 0,12, а для сплава ПТ-7М эмпирический коэффициент k от 0,02 до менее 0,15, ε – логарифмическая степень деформации; υ<sub>ПР</sub> – скорость перемещения деформирующего инструмента при прессовании, мм/с. Холодную прокатку осуществляют со степенью деформации от 40 до 44% с использованием жидких технологических смазок, а промежуточные термические обработки проводят в вакууме при температуре 670-690°С в течение 120 мин для сплава ПТ-1М или при температуре 730-790°С в течение 120 мин для ПТ-7М. Конечную термическую обработку труб готового размера проводят в вакууме при температуре 670-690°С в течение 120 мин для сплава ПТ-1М или при температуре 730-790°С в течение 120 мин для ПТ-7М. Обеспечивается получение требуемых механических свойств труб, увеличение коэффициента выхода годного за счет отсутствия дефектов на поверхности холоднодеформированных труб. 1 з.п. ф-лы, 5 ил. | ru |
dc.description.abstract | FIELD: metallurgy. SUBSTANCE: invention relates to metallurgy, namely, to the manufacture of weldless cold-worked pipes from titanium alloys, and can be used for manufacturing heavy-duty articles. Method for manufacturing cold-worked weldless pipes from titanium alloys includes machining hot-worked cylindrical workpieces, pressing, levelling, and machining the resulting hot-pressed pipes, followed by multi-pass cold rolling while performing intermediate heat treatments in vacuum, depending on the alloy, and finishing heat treatment of pipes of the finished size in vacuum. The PT-1M or PT-7M alloy is used as titanium alloys for the pipes; prior to heating for pressing, a protective coating is applied to the surface of the workpieces, constituting a slip coat consisting of a mixture of powdered EVT-24 enamel, ground bentonite clay, and liquid glass. Pressing is then performed at a temperature T<sub>H</sub> determined by the dependence: T<sub>H</sub> = T<sub>PP</sub> – k·ε·υ<sub>PR</sub>, wherein T<sub>PP</sub> is the polymorphic transition temperature, °C; k is an empirical coefficient accounting for the influence of deformation heat-up, °C·s/mm; for the PT-1M alloy, the empirical coefficient k is from 0.035 to 0.12, and for the PT-7M alloy, the empirical coefficient k is from 0.02 to less than 0.15, ε is the logarithmic degree of deformation; υ<sub>PR</sub> is the rate of movement of the deforming tool during pressing, mm/s. Cold rolling is performed with a 40 to 44% degree of deformation, using liquid process lubricants; and intermediate heat treatments are performed in vacuum at a temperature of 670 to 690°C for 120 minutes for the PT-1M alloy or at 730 to 790°C for 120 minutes for the PT-7M alloy. The finishing heat treatment of pipes of the finished size is performed in vacuum at a temperature of 670 to 690°C for 120 minutes for the PT-1M alloy or at 730 to 790°C for 120 minutes for the PT-7M alloy. EFFECT: required mechanical properties of the pipes are obtained, and yield coefficient is increased due to the absence of defects on the surface of cold-worked pipes. 2 cl, 5 dwg. | en |
dc.format.mimetype | application/pdf | en |
dc.language.iso | ru | en |
dc.relation | https://www.fips.ru/registers-doc-view/fips_servlet?DB=RUPAT&DocNumber=2778319&TypeFile=html | fips |
dc.subject | PATENT | en |
dc.subject | INVENTION | en |
dc.subject | ПАТЕНТЫ | ru |
dc.subject | ИЗОБРЕТЕНИЯ | ru |
dc.subject.other | 530000 | grnti |
dc.subject.other | C22F 1/18 | mpk |
dc.subject.other | B21B 3/00 | mpk |
dc.subject.other | B21B 21/00 | mpk |
dc.subject.other | B21J 5/00 | mpk |
dc.title | Способ изготовления холоднодеформированных бесшовных труб из титановых сплавов | ru |
dc.title.alternative | Method for Manufacturing Cold-Worked Weldless Pipes from Titanium Alloys | en |
dc.type | Patent | en |
dc.type | info:eu-repo/semantics/patent | en |
dc.identifier.rsi | 49316523 | - |
local.patent.datepriotity | 2021-04-29 | appldate |
local.patent.datepriotity | 2021112431 | applnumber |
local.patent.number | 2778319 | - |
local.patent.owner | Ural Federal University | en |
local.patent.owner | Федеральное государственное автономное образовательное учреждение высшего образования «Уральский федеральный университет имени первого Президента России Б.Н. Ельцина» | ru |
local.patent.type | Патент на изобретение | ru |
local.patent.country | RUS | en |
local.identifier.pure | 46444190 | - |
Располагается в коллекциях: | Патенты и изобретения |
Файлы этого ресурса:
Файл | Описание | Размер | Формат | |
---|---|---|---|---|
2778319.PDF | 5,53 MB | Adobe PDF | Просмотреть/Открыть |
Все ресурсы в архиве электронных ресурсов защищены авторским правом, все права сохранены.