Title: Non-crystallising Glass Sealants for SOFC: Effect of Y2O3 Addition
Authors: Krainova, D. A.
Saetova, N. S.
Kuzmin, A. V.
Raskovalov, A. A.
Eremin, V. A.
Ananyev, M. V.
Steinberger-Wilckens, R.
Issue Date: 2020
Publisher: Elsevier Ltd
Elsevier BV
Citation: Non-crystallising Glass Sealants for SOFC: Effect of Y2O3 Addition / D. A. Krainova, N. S. Saetova, A. V. Kuzmin et al. — DOI 10.1039/d1ra07440g // Ceramics International. — 2020. — Vol. 46. — Iss. 4. — P. 5193-5200.
Abstract: The joining of ceramic and metal (interconnect) parts is one of the main challenges in the development of solid oxide fuel cells (SOFC). A promising approach to solving this problem is the use of glassy sealants. In this work, we investigated the effect of yttria additions on the properties of SiO2–Al2O3–CaO–Na2O–ZrO2–Y2O3 glass sealants. An increase in the concentration of yttria is shown to reduce the tendency of the glasses under study to crystallisation. A glass containing 4 wt% of Y2O3 is found to be amorphous, even after exposure at 850 °C for 100 h. Moreover, the defectiveness of the glass microstructure, after sealing, is found to decrease along with a growth in the Y2O3 concentration. The developed non-crystallising sealant was successfully applied for joining a YSZ ceramic and an Fe–Ni–Co alloy having the phase transition of around 500 °C. The use of the non-crystallising sealant allows us to join materials with very different thermal expansion coefficients and to avoid cracking under cooling, which might occur due to a large difference in thermal expansion coefficients. © 2019 Elsevier Ltd and Techna Group S.r.l.
Keywords: CRYSTALLISATION
GLASS SEALANT
NON-CRYSTALLISING SEALANT
SEALING MICROSTRUCTURE
SOFC
ALUMINA
ALUMINUM OXIDE
CERAMIC MATERIALS
COBALT ALLOYS
CRYSTALLIZATION
EXPANSION
GLASS
JOINING
MICROSTRUCTURE
SEALANTS
SILICA
SODIUM COMPOUNDS
THERMAL EXPANSION
YTTRIA STABILIZED ZIRCONIA
YTTRIUM OXIDE
ZIRCONIA
CO ALLOYS
GLASS MICROSTRUCTURE
GLASS SEALANTS
JOINING OF CERAMICS
THERMAL EXPANSION COEFFICIENTS
YSZ CERAMICS
SOLID OXIDE FUEL CELLS (SOFC)
URI: http://elar.urfu.ru/handle/10995/111827
Access: info:eu-repo/semantics/openAccess
SCOPUS ID: 85074146512
PURE ID: 11888841
ISSN: 0272-8842
DOI: 10.1039/d1ra07440g
metadata.dc.description.sponsorship: This study was financially supported by the RFBR project no. 17-58-10006. The research was partially performed using the facilities of the Shared Access Centre “Composition of Compounds” of IHTE UB RAS . The authors are grateful to Dr. S.V. Plaksin for XRD analysis, Dr. N. I. Moskalenko for AES analysis, A. S. Farlenkov for SEM analysis, and A. A. Solodyankin and V. A. Vorotnikov for their assistance in sample preparation.
Appears in Collections:Научные публикации ученых УрФУ, проиндексированные в SCOPUS и WoS CC

Files in This Item:
File Description SizeFormat 
2-s2.0-85074146512.pdf954,28 kBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.