Пожалуйста, используйте этот идентификатор, чтобы цитировать или ссылаться на этот ресурс: http://elar.urfu.ru/handle/10995/127216
Полная запись метаданных
Поле DCЗначениеЯзык
dc.contributor.authorРычков, В. Н.ru
dc.contributor.authorМашковцев, М. А.ru
dc.contributor.authorЗацепин, А. Ф.ru
dc.contributor.authorКузнецова, Ю. А.ru
dc.contributor.authorГаврилов, Н. В.ru
dc.contributor.authorМамонов, А. П.ru
dc.contributor.authorRychkov, V. N.en
dc.contributor.authorMashkovtsev, M. A.en
dc.contributor.authorZatsepin, A. F.en
dc.contributor.authorKuznetsova, Iu. A.en
dc.contributor.authorGavrilov, N. V.en
dc.contributor.authorMamonov, A. P.en
dc.date.accessioned2023-10-10T08:19:49Z-
dc.date.available2023-10-10T08:19:49Z-
dc.date.issued2022-05-25-
dc.identifier.urihttp://elar.urfu.ru/handle/10995/127216-
dc.description.abstractИзобретение относится к области технологии функциональных материалов и устройств нанофотоники, оптоэлектроники и конвертеров излучения с высокой термической стабильностью на базе наноразмерных тонкопленочных структур оксидов редкоземельных элементов. Способ получения оптического тонкопленочного покрытия из оксида гадолиния Gd<sub>2</sub>O<sub>3</sub> на подложке из кварцевого стекла методом высокочастотного реакционного магнетронного распыления включает следующие операции. Предварительно из порошка металлического гадолиния с размером частиц от 5 до 20 мкм изготавливают мишень для распыления методом холодного прессования при давлении прессования от 10 до 50 МПа. Наносят покрытие из оксида гадолиния на поверхность упомянутой подложки в течение 5-6 ч при мощности магнетронного разряда от 100 до 200 Вт в аргон-кислородной среде c общим давлением 0,15 Па при объемной концентрации кислорода от 25 до 35%. В процессе нанесения температуру подложки поддерживают 150-250°С. После нанесения упомянутого покрытия подложку из кварцевого стекла с нанесенным покрытием из оксида гадолиния в виде тонкой пленки охлаждают в вакуумной камере при общем давлении не выше 10<sup>-3</sup> Па до комнатной температуры. Обеспечивается повышение степени однородности и увеличение диапазона спектральной прозрачности до 5,5 эВ оптических тонкопленочных покрытий на основе оксида гадолиния Gd<sub>2</sub>O<sub>3</sub> на подложке из кварцевого стекла. 5 пр., 3 ил.ru
dc.description.abstractFIELD: functional materials technology. SUBSTANCE: invention relates to the field of technology of functional materials and devices for nanophotonics, optoelectronics and radiation converters with high thermal stability based on nanosized thin-film structures of oxides of rare earth elements. The method for producing an optical thin film coating of gadolinium oxide Gd<sub>2</sub>O<sub>3</sub> on a quartz glass substrate by high-frequency reactive magnetron sputtering includes the following steps. A target for sputtering is preliminarily made from gadolinium metal powder with a particle size of 5 to 20 mcm by cold pressing at a pressing pressure of 10 to 50 MPa. A coating of gadolinium oxide is applied to the surface of said substrate for 5-6 hours at a magnetron discharge power of 100 to 200 W in an argon-oxygen medium with a total pressure of 0.15 Pa at an oxygen volume concentration of 25 to 35%. During application, the temperature of the substrate is maintained at 150-250°C. After applying said coating, the quartz glass substrate coated with gadolinium oxide in the form of a thin film is cooled in a vacuum chamber at a total pressure of not more than 10-3 Pa to room temperature. EFFECT: increase in the degree of homogeneity and increase in the range of spectral transparency up to 5.5 eV of optical thin-film coatings based on gadolinium oxide Gd<sub>2</sub>O<sub>3</sub> on a quartz glass substrate. 1 cl, 5 ex, 3 dwg.en
dc.format.mimetypeapplication/pdfen
dc.language.isoruen
dc.relationhttps://www.fips.ru/registers-doc-view/fips_servlet?DB=RUPAT&DocNumber=2772770&TypeFile=htmlfips
dc.subjectPATENTen
dc.subjectINVENTIONen
dc.subjectПАТЕНТЫru
dc.subjectИЗОБРЕТЕНИЯru
dc.subject.other552200grnti
dc.subject.otherC23C 14/08mpk
dc.subject.otherC23C 14/18mpk
dc.subject.otherC23C 14/35mpk
dc.subject.otherB22F 3/02mpk
dc.titleСпособ получения оптических тонкопленочных функциональных покрытий Gd2O3 на подложке кварцевого стеклаru
dc.title.alternativeMethod for Producing Optical Thin-Film Gd2O3 Functional Coatings on a Quartz Glass Substrateen
dc.typePatenten
dc.typeinfo:eu-repo/semantics/patenten
dc.identifier.rsi48770780-
local.patent.datepriotity2021-12-22appldate
local.patent.datepriotity2021138147applnumber
local.patent.number2772770-
local.patent.ownerФедеральное государственное автономное образовательное учреждение высшего образования «Уральский федеральный университет имени первого Президента России Б.Н. Ельцина»ru
local.patent.ownerUral Federal Universityen
local.patent.typeПатент на изобретениеru
local.patent.countryRUSen
Располагается в коллекциях:Патенты и изобретения

Файлы этого ресурса:
Файл Описание РазмерФормат 
2772770.PDF1,26 MBAdobe PDFПросмотреть/Открыть